Exterior paint peels on houses in Leavenworth, KS, and across Kansas, mostly because water gets behind the paint, and a new coat will fail the same way until the source of that water is fixed. Other causes include wood that weathered before it was painted, old paint that was dirty or chalky when the new coat went on, and too many layers of paint. This guide shows how to tell which one you have.
Peeling to bare wood: find the water first
The USDA Forest Products Laboratory puts it simply: all decay, and most exterior paint failures, start with moisture. Paint only slows the penetration of water; it does not stop it. When paint peels all the way to bare wood, the National Park Service says the cause is most often excess moisture collecting behind the paint film, from outside or inside the house. Its advice is blunt: there is no sense in repainting before dealing with the moisture, because new paint will simply fail.
Outside sources to check, from the Park Service's list:
- faulty flashing
- leaking gutters
- defective roof shingles
- cracks and holes in siding and trim
- deteriorated caulking in joints and seams
- shrubbery growing too close to painted wood
The Forest Products Laboratory's 1976 research note adds inadequate vapor barriers, ice dams, leaky roofs and poor gutters and downspouts, and its Wood Handbook adds condensation from inside the house, often from bathrooms or kitchens. The Park Service's fix for moisture from inside is exhaust fans and vents. Once the source is fixed, the wood has to dry out thoroughly before it is painted again.
Blisters: water or heat?
Cut a blister open and look underneath.
- Bare wood underneath points to water. Water blisters form between the wood and the primer. The Forest Products Laboratory finds them on siding and trim where rain gets in through improperly flashed doors, windows and vents, near unsealed end grain, and below ice dams and overflowing gutters. Oil-based paint is more prone to them than latex paint.
- Another layer of paint underneath points to heat. This is solvent blistering, which the Park Service says happens when paint goes on in direct sunlight and the surface dries too fast. It is more common with dark colors.
Wrinkling is a related problem. The Park Service traces it to paint applied too thick, a second coat put on before the first was dry, too little brushing out, or painting in temperatures higher than the manufacturer recommends. Our guide to when to paint a house exterior in Leavenworth covers the weather side of both.
Peeling between coats
Sometimes the new paint lets go of the old paint rather than the wood. The Forest Products Laboratory says this intercoat peeling usually occurs within a year of repainting, and the way to prevent it is to make sure the old paint is clean. The Park Service says it most often happens in protected areas such as eaves and covered porches, which never get a regular rinsing from the rain. It also happens where paints do not match: latex over old, chalking oil paint may not adhere. A quality oil-type exterior primer gives a surface that either an oil or a latex topcoat can go over.
A tape test catches the problem before it happens. Paint a small, hidden area and let it dry at least overnight. Press on a strip of strongly adhering tape and pull it off. If both the new and the old paint come off on the tape, the old paint is not well bonded and has to be removed before the house is repainted.
Paint over weathered wood
Bare wood left in the sun before painting is a major cause of coating failures, according to the Forest Products Laboratory. In its test on cedar boards finished with a primer and two latex topcoats, boards left bare in the sun for 16 weeks peeled and needed refinishing within 3 years. Boards bare for 1 week started peeling after 13 years. Boards never exposed were still in good condition after 20.
Wood that looks weathered and silver or gray is badly degraded, and it needs sanding to sound wood before a paint film will stick. The tape test works here too: press strong tape on the bare wood and snap it off, and if wood fibers come away with it, paint will peel there.
New, smooth siding has its own suspect. Mill glaze is often blamed when paint peels off it, but the laboratory's scientists could not reproduce mill glaze and found the real causes were raised grain, wood that weathered before it was painted, and moisture.
Too many layers: cracking and alligatoring
On older houses the problem can be too much paint. The Park Service says that when paint builds up to about 1/16 inch, roughly 16 to 30 layers, one or more extra coats may be enough to trigger cracking and peeling, and that thick paint fails at the oldest layers, next to the wood. Crazing, the fine interconnected breaks that form in the top layer as old paint grows hard and brittle, becomes cracking and alligatoring if it is left alone. The Forest Products Laboratory adds that cross-grain cracking usually occurs on houses with thick layers of old oil-alkyd paint, and the fix is removing the old paint in those areas.
Repainting too often feeds the problem. The 1976 research note warns that repainting too frequently can build a paint film thick enough to fail, and the 2021 Wood Handbook says not to paint too often, because too many coats of latex can eventually lead to adhesion failure of the primer. If your house is old enough to carry decades of paint, our page on historic home exterior painting covers how much to take off and how.
Board ends, sills and other places peeling starts
Peeling and flaking are often worst at the ends of boards, because liquid water enters wood 10 to 100 times faster through end grain than through the other faces. Horizontal surfaces such as window sills deteriorate faster than walls and need repainting more often. Finger-jointed fascia and trim often fail in a patchwork pattern at the joints. When peeling starts in these places and nowhere else, the trim may need attention before the walls do. See trim, fascia and soffit painting.
Stains and mildew that look like paint failure
Not every bad-looking wall has failed paint.
- Brown or reddish stains on cedar or redwood are often extractives, carried to the surface by water. Another coat of the same paint will not stop them. The Forest Products Laboratory's fix is a stain-blocking primer, then a new topcoat, after the water source is dealt with.
- Stains around nail heads come from rusting nails, the Park Service notes.
- Dark spots may be dirt or mildew. Put a drop of household bleach on the spot: mildew turns white, and dirt stays dirt.
Mildew grows where moisture stays longest and sun is scarce: window sills, under eaves, around gutters and downspouts, on the north side and near shrubbery. Sound paint with mildew on it is washed, not repainted. The Park Service's cleaning mix for mildew on painted wood is one cup of non-ammoniated detergent, one quart of household bleach and one gallon of water. The Park Service also notes that cleaning quite often gives a good enough result to postpone repainting.
Match the fix to the failure
The Park Service's three classes of paint condition turn the diagnosis into a plan:
| What you see | Class | The fix |
|---|---|---|
| Dirt, soot, mildew, heavy chalking, stains | Class I | Clean it; generally no paint removal |
| Crazing, peeling between coats, heat blisters, wrinkling | Class II | Scrape and sand to the next sound layer |
| Peeling to bare wood, cracking, alligatoring | Class III | Fix the water, then remove the paint in the affected areas, prime and repaint |
For the steps in order, see our guide to preparing wood siding for paint, or our wood siding painting page if you would rather have it done.
Lead precautions before anyone scrapes
On a house built before 1978, old or worn lead-based paint can produce chips and dust, and paid work that scrapes or sands it falls under EPA's lead renovation rule, which Kansas runs through its own program. Read our lead paint guide before anyone, including you, starts scraping.
Peeling paint questions
Will new paint stop the peeling?
No, not until the water is fixed. The Park Service says there is no sense in repainting before dealing with the moisture, because new paint will simply fail. Find the leak, let the wood dry, then repaint.
Why is paint peeling on only one side of my house?
That side has the water or the sun. Check its gutters, flashing and caulk, any shrubs against the wall, and what is on the inside of that wall, such as a bathroom or kitchen. A sunny side also wears out faster, since paint on a shaded side often lasts twice as long.
Why did my paint peel a year after repainting?
The new coat did not bond to the old one. That intercoat peeling usually shows up within a year and usually traces back to old paint that was dirty or chalky when the new coat went on. The fix is removing the loose paint and cleaning the old surface thoroughly before the next coat.
How can I tell mildew from dirt?
Use a drop of household bleach: mildew turns white, and dirt stays dirt. Sound paint with mildew on it needs washing, not repainting.
Sources
- National Park Service, Preservation Brief 10: Exterior Paint Problems on Historic Woodwork, September 1982, read November 26, 2026
- USDA Forest Service, Forest Products Laboratory, Wood Handbook, Chapter 16: Finishing Wood, General Technical Report FPL-GTR-282, 2021, read November 26, 2026
- USDA Forest Service, Forest Products Laboratory, Research Note FPL-0232: How to Refinish Wood Siding with Latex Paints, 1976, read November 26, 2026
- U.S. Environmental Protection Agency, Lead Renovation, Repair and Painting Program, read November 26, 2026
Send photos of the peeling
Send close photos of the peeling, a wide photo of that side of the house and a photo of the gutters above it. Get a Quote